Multi-Pass Laser and Hybrid Laser-Arc Narrow-Gap Welding of Steel Butt Joints

التفاصيل البيبلوغرافية
Parent link:Materials Science Forum: Scientific Journal
Vol. 927 : Materials and Processing Technology II.— 2018.— [P. 64-71]
مؤلف مشترك: Национальный исследовательский Томский политехнический университет (ТПУ) Юргинский технологический институт (филиал) (ЮТИ) Кафедра сварочного производства (КСП)
مؤلفون آخرون: Shelyagin V., Khaskin V., Bernatskyi A., Siora A., Sydorets V. N. Volodymyr, Chinakhov D. A. Dmitriy Anatol'evich
الملخص:Title screen
Multi-pass laser and laser-arc narrow-gap welding make it possible to obtain high-quality butt joints of large-thickness pipe steels with hardness up to 2600...2800 MPa and toughness close to the base metal toughness at a temperature of 20°C. When multi-pass welding methods are used, the subsequent pass makes heat treatment of the previous ones, and reduces the rate of their cooling yet. This allows excluding heat treatment of the joint after welding, which significantly reduces the time and costs for manufacturing large-sized structures.
Режим доступа: по договору с организацией-держателем ресурса
اللغة:الإنجليزية
منشور في: 2018
الموضوعات:
الوصول للمادة أونلاين:https://doi.org/10.4028/www.scientific.net/MSF.927.64
التنسيق: الكتروني فصل الكتاب
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=658528