Specifics of Welded Joint Destruction Obtained by Friction Stir Welding at Strain
| Parent link: | Applied Mechanics and Materials: Scientific Journal Vol. 756 : Mechanical Engineering, Automation and Control Systems (MEACS2014).— 2015.— [P. 137-143] |
|---|---|
| Corporate Author: | |
| Other Authors: | , , , |
| Summary: | Title screen The specifics of fracture of weld seam samples of aluminium-magnesium alloy, obtained by the friction stir welding (FSW) method at strain, have been studied. It has been shown that the weld seam contains aluminium-oxides, which are located on the surface of the conjugation of two sample parts. This imperfection leads to the effect when the initial crack spreads from the seam root over this surface of conjugation. The subsequent fracture proceeds over the basic metal of the seam. Режим доступа: по договору с организацией-держателем ресурса |
| Published: |
2015
|
| Series: | Mechanical Engineering, Processing and Surface Engineereng, Metals Treatment, Equipment and Tools |
| Subjects: | |
| Online Access: | http://dx.doi.org/10.4028/www.scientific.net/AMM.756.137 |
| Format: | Electronic Book Chapter |
| KOHA link: | https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=641295 |