Synthesis of Photoluminophors Using a Continuous Solid-phase Technology; Procedia Chemistry; Vol. 11 : 1st International Symposium on Inorganic Fluorides: Chemistry and Technology, ISIF 2014, Tomsk, Russia
| Источник: | Procedia Chemistry Vol. 11 : 1st International Symposium on Inorganic Fluorides: Chemistry and Technology, ISIF 2014, Tomsk, Russia.— 2014.— [P. 152-157] |
|---|---|
| Автор-организация: | |
| Другие авторы: | , , , , |
| Примечания: | Title screen Solid phase method of strontium aluminate synthesis (SrAl[2]O[4]) is based on calcination of the mixture of strontium carbonate (SrCO[3]), aluminum oxide (Al[2][O[3]), oxides of REM (europium, dysprosium) and a mineralizer - borate glass (H[3]BO[3]) at a temperature of 1200-1400 °C within 4-6 hours. We have proposed a technique of thermal shock – rapid heating and rapid cooling of the sample by means of which the duration of synthesis is reduced to 30 minutes. Режим доступа: по договору с организацией-держателем ресурса |
| Язык: | английский |
| Опубликовано: |
2014
|
| Предметы: | |
| Online-ссылка: | http://dx.doi.org/10.1016/j.proche.2014.11.027 |
| Формат: | Электронный ресурс Статья |
| Запись в KOHA: | https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=639625 |
| Примечания: | Title screen Solid phase method of strontium aluminate synthesis (SrAl[2]O[4]) is based on calcination of the mixture of strontium carbonate (SrCO[3]), aluminum oxide (Al[2][O[3]), oxides of REM (europium, dysprosium) and a mineralizer - borate glass (H[3]BO[3]) at a temperature of 1200-1400 °C within 4-6 hours. We have proposed a technique of thermal shock – rapid heating and rapid cooling of the sample by means of which the duration of synthesis is reduced to 30 minutes. Режим доступа: по договору с организацией-держателем ресурса |
|---|---|
| DOI: | 10.1016/j.proche.2014.11.027 |