The porosity and nuclear magnetic characteristics of artificial samples with the equal grain size; Известия Томского политехнического университета [Известия ТПУ]. Инжиниринг георесурсов; Т. 336, № 5

Dades bibliogràfiques
Parent link:Известия Томского политехнического университета [Известия ТПУ]. Инжиниринг георесурсов=Bulletin of the Tomsk Polytechnic University. Geo Assets Engineering/ Национальный исследовательский Томский политехнический университет.— .— Томск: Изд-во ТПУ, 2015-.— 2413-1830
Т. 336, № 5.— 2025.— P. 110-119
Autor principal: Timofey A. Yanushenko
Altres autors: Nikita A. Golikov
Sumari:Relevance. The nuclear magnetic resonance relaxometry is a fairly new method for well logging and laboratory investigations. It is applied for determining petrophysical properties, e.g., porosity, permeability, water- and oil-saturation. However, the nuclear magnetic resonance relaxometry data interpretation rests on the representation of the pore space as a set of spheres of various diameters that fundamentally does not correspond to the structure of granular rocks. Aim. To examine an influence of grain size on the measurements results of nuclear magnetic resonance relaxometry porosity and compare with other conventional methods. Objects. Artificial samples made with various sand and quartz glass beads fractions. Methods. Water-saturation, gas-volumetric and nuclear magnetic resonance relaxometry were applied to determine porosity. X-ray diffraction method was used to clarify the mineralogical composition; to measure the grain size a laser particle size analyzer was used, and the grain shape was investigated in polished specimens. Results. The paper describes the results of porosity measurements with different methods for artificial samples. We observed an effect of underestimated porosity acquired with nuclear magnetic resonance relaxometry method for consolidated and unconsolidated samples with grain size less than 0.160 mm. The investigation of sand composition with the X-ray diffraction method and additional assessment of the particles shape and size led to conclude that these factors are not the cause of the underestimated porosity effect. Additional statistical samples and using of the other nuclear magnetic resonance relaxometer presented the reparability of previous results. Based on the research results, it was assumed that the cause of the underestimated porosity effect is the complex shape and increased specific surface area of the samples, which grows as the particle size decreases
Актуальность. Ядерно-магнитная резонансная релаксометрия является относительно новым методом каротажа и лабораторных исследований. Он применяется для определения петрофизических свойств, например, таких как, пористость, проницаемость, насыщенность водой и нефтью. Однако интерпретация данных ядерномагнитной резонансной релаксометрии подразумевает представление порового пространства как набора сфер различного диаметра, что не соответствует структуре терригенных пород. Целью исследования было изучение влияния размера зерна на результаты измерения пористости ядерно-магнитной резонансной релаксометрией и сопоставление с другими стандартными методами. Объектом исследования являются искусственные образцы из различных фракций песка и стеклянных кварцевых шариков. Методы. Для определения пористости применяли метод жидкостенасыщения, газоволюметрический метод и ядерно-магнитную резонансную релаксометрию. Рентгенофазовый метод использовался для уточнения минералогического состава; для оценки размера зерен применялся лазерный анализатор размеров частиц, форма зерен исследовалась в шлифах. Результаты. Описаны результаты измерений пористости различными методами на искусственных образцах. Мы наблюдали эффект занижения пористости, измеренный методом ЯМР для консолидированных и неконсолидированных образцов с размером зерна менее 0,160 мм. Исследование состава песка рентгенофазовым методом и дополнительная оценка формы и размера зерен позволили сделать вывод, что эти факторы не являются причиной данного эффекта. Дополнительные статистические выборки и использование другого ЯМР-релаксометра подтвердили повторяемость предыдущих результатов. По результатам исследований сделано предположение, что причиной эффекта занижения пористости является сложная форма и повышенная удельная поверхность зерен образцов, которая увеличивается с уменьшением размера зерен
Текстовый файл
Idioma:anglès
Publicat: 2025
Matèries:
Accés en línia:https://earchive.tpu.ru/handle/11683/123528
https://doi.org/10.18799/24131830/2025/5/4723
Format: Electrònic Capítol de llibre
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=680523

MARC

LEADER 00000naa2a2200000 4500
001 680523
005 20250618103422.0
090 |a 680523 
100 |a 20250609d2025 k||y0rusy50 ba 
101 0 |a eng 
102 |a RU 
135 |a drcn uucaa 
200 1 |a The porosity and nuclear magnetic characteristics of artificial samples with the equal grain size  |d Пористость и ядерно-магнитные характеристики искусственных образцов с одинаковым размером зерен  |z rus  |f Timofey A. Yanushenko, Nikita A. Golikov 
320 |a References: p. 117-118 (26 tit.) 
330 |a Relevance. The nuclear magnetic resonance relaxometry is a fairly new method for well logging and laboratory investigations. It is applied for determining petrophysical properties, e.g., porosity, permeability, water- and oil-saturation. However, the nuclear magnetic resonance relaxometry data interpretation rests on the representation of the pore space as a set of spheres of various diameters that fundamentally does not correspond to the structure of granular rocks. Aim. To examine an influence of grain size on the measurements results of nuclear magnetic resonance relaxometry porosity and compare with other conventional methods. Objects. Artificial samples made with various sand and quartz glass beads fractions. Methods. Water-saturation, gas-volumetric and nuclear magnetic resonance relaxometry were applied to determine porosity. X-ray diffraction method was used to clarify the mineralogical composition; to measure the grain size a laser particle size analyzer was used, and the grain shape was investigated in polished specimens. Results. The paper describes the results of porosity measurements with different methods for artificial samples. We observed an effect of underestimated porosity acquired with nuclear magnetic resonance relaxometry method for consolidated and unconsolidated samples with grain size less than 0.160 mm. The investigation of sand composition with the X-ray diffraction method and additional assessment of the particles shape and size led to conclude that these factors are not the cause of the underestimated porosity effect. Additional statistical samples and using of the other nuclear magnetic resonance relaxometer presented the reparability of previous results. Based on the research results, it was assumed that the cause of the underestimated porosity effect is the complex shape and increased specific surface area of the samples, which grows as the particle size decreases 
330 |a Актуальность. Ядерно-магнитная резонансная релаксометрия является относительно новым методом каротажа и лабораторных исследований. Он применяется для определения петрофизических свойств, например, таких как, пористость, проницаемость, насыщенность водой и нефтью. Однако интерпретация данных ядерномагнитной резонансной релаксометрии подразумевает представление порового пространства как набора сфер различного диаметра, что не соответствует структуре терригенных пород. Целью исследования было изучение влияния размера зерна на результаты измерения пористости ядерно-магнитной резонансной релаксометрией и сопоставление с другими стандартными методами. Объектом исследования являются искусственные образцы из различных фракций песка и стеклянных кварцевых шариков. Методы. Для определения пористости применяли метод жидкостенасыщения, газоволюметрический метод и ядерно-магнитную резонансную релаксометрию. Рентгенофазовый метод использовался для уточнения минералогического состава; для оценки размера зерен применялся лазерный анализатор размеров частиц, форма зерен исследовалась в шлифах. Результаты. Описаны результаты измерений пористости различными методами на искусственных образцах. Мы наблюдали эффект занижения пористости, измеренный методом ЯМР для консолидированных и неконсолидированных образцов с размером зерна менее 0,160 мм. Исследование состава песка рентгенофазовым методом и дополнительная оценка формы и размера зерен позволили сделать вывод, что эти факторы не являются причиной данного эффекта. Дополнительные статистические выборки и использование другого ЯМР-релаксометра подтвердили повторяемость предыдущих результатов. По результатам исследований сделано предположение, что причиной эффекта занижения пористости является сложная форма и повышенная удельная поверхность зерен образцов, которая увеличивается с уменьшением размера зерен 
336 |a Текстовый файл 
461 1 |0 288378  |9 288378  |t Известия Томского политехнического университета [Известия ТПУ]. Инжиниринг георесурсов  |l Bulletin of the Tomsk Polytechnic University. Geo Assets Engineering  |f Национальный исследовательский Томский политехнический университет  |c Томск  |n Изд-во ТПУ  |d 2015-   |x 2413-1830 
463 1 |0 680495  |9 680495  |t Т. 336, № 5  |d 2025  |v P. 110-119 
610 1 |a electronic resource 
610 1 |a porosity 
610 1 |a grain size 
610 1 |a artificial samples 
610 1 |a petrophysical properties 
610 1 |a nuclear magnetic resonance relaxometry 
610 1 |a gasvolumetric method 
610 1 |a water-saturating method 
610 1 |a пористость 
610 1 |a размер зерен 
610 1 |a искусственные образцы 
610 1 |a петрофизические свойства 
610 1 |a ядерно-магнитная резонансная (ЯМР) релаксометрия 
610 1 |a газоволюметрический метод 
610 1 |a метод жидкостенасыщения 
700 1 |a Timofey A. Yanushenko 
701 1 |a Nikita A. Golikov 
801 0 |a RU  |b 63413507  |c 20250609 
850 |a 63413507 
856 4 |u https://earchive.tpu.ru/handle/11683/123528  |z https://earchive.tpu.ru/handle/11683/123528 
856 4 |u https://doi.org/10.18799/24131830/2025/5/4723  |z https://doi.org/10.18799/24131830/2025/5/4723 