| Parent link: | Курзина, И. А. (химик ; 1972-). Перспективы развития фундаментальных наук=Prospects of Fundamental Sciences Development: сборник научных трудов XX Международной конференции студентов, аспирантов и молодых ученых, г. Томск, 25-28 апреля 2023 г..— .— Томск: Изд-во ТПУ, 2023 Т. 1 : Физика.— 2023.— С. 327-329 |
|---|---|
| Main Author: | |
| Corporate Author: | |
| Other Authors: | |
| Summary: | Заглавие с экрана Thin (1.3 μm) and thick (13.0 μm) multilayer Cr/Al2O3 coatings were deposited onto E110 zirconium alloy using magnetron sputtering of Cr and Al targets in Ar and Ar+O2 atmospheres, respectively. Oxidation tests of thin coatings were performed in air at 1100 °C for 5-20 min. The high-temperature oxidation of thick coatings were done at 1200-1400 °C in a water steam. The resistance to oxidation in air and water steam is discussed in the paper Текстовый файл |
| Published: |
2023
|
| Subjects: | |
| Online Access: | http://earchive.tpu.ru/handle/11683/80826 |
| Format: | Electronic Book Chapter |
| KOHA link: | https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=673516 |
MARC
| LEADER | 00000naa2a2200000 4500 | ||
|---|---|---|---|
| 001 | 673516 | ||
| 005 | 20241101144732.0 | ||
| 090 | |a 673516 | ||
| 100 | |a 20240703d2023 k||y0rusy50 ca | ||
| 101 | 0 | |a rus | |
| 102 | |a RU | ||
| 135 | |a drcn ---uucaa | ||
| 200 | 1 | |a Защитные многослойные Cr/Al2O3 покрытия для циркониевых сплавов от высокотемпературного окисления |f С. Е. Ручкин |g науч. рук. Д. В. Сиделёв ; Инженерная школа ядерных технологий НИ ТПУ |d Protective multilayer Cr/Al2O3 coatings for zirconium alloys from high-temperature oxidation |z eng | |
| 300 | |a Заглавие с экрана | ||
| 320 | |a Библиография: с. 329 | ||
| 330 | |a Thin (1.3 μm) and thick (13.0 μm) multilayer Cr/Al2O3 coatings were deposited onto E110 zirconium alloy using magnetron sputtering of Cr and Al targets in Ar and Ar+O2 atmospheres, respectively. Oxidation tests of thin coatings were performed in air at 1100 °C for 5-20 min. The high-temperature oxidation of thick coatings were done at 1200-1400 °C in a water steam. The resistance to oxidation in air and water steam is discussed in the paper | ||
| 336 | |a Текстовый файл | ||
| 461 | 1 | |0 636133 |t Перспективы развития фундаментальных наук |l Prospects of Fundamental Sciences Development |o сборник научных трудов XX Международной конференции студентов, аспирантов и молодых ученых, г. Томск, 25-28 апреля 2023 г. |d 2023 |9 636133 |a Курзина, И. А. (химик ; 1972-) |c Томск |n Изд-во ТПУ | |
| 463 | 1 | |0 669915 |t Т. 1 : Физика |v С. 327-329 |d 2023 |9 669915 |p 1 файл (75,9 MB, 442 с.) |u conference_tpu-2023-C21_V1.pdf |l Volume 1. Physics | |
| 610 | 1 | |a труды учёных ТПУ | |
| 610 | 1 | |a электронный ресурс | |
| 610 | 1 | |a энергетические реакторы | |
| 610 | 1 | |a толерантное топливо | |
| 610 | 1 | |a защитное покрытие | |
| 610 | 1 | |a циркониевые оболочки | |
| 610 | 1 | |a ионно-плазменная установка | |
| 610 | 1 | |a магнетроны | |
| 610 | 1 | |a высокотемпературное окисление | |
| 610 | 1 | |a циркониевые образцы | |
| 700 | 1 | |a Ручкин |b С. Е. | |
| 702 | 1 | |a Сиделёв |b Д. В. |c физик |c инженер кафедры Томского политехнического университета |f 1991- |g Дмитрий Владимирович |4 727 | |
| 712 | 0 | 2 | |a Национальный исследовательский Томский политехнический университет |b Инженерная школа ядерных технологий |b Отделение экспериментальной физики |9 28346 |
| 801 | 0 | |a RU |b 63413507 |c 20240703 |g RCR | |
| 856 | 4 | |z http://earchive.tpu.ru/handle/11683/80826 |u http://earchive.tpu.ru/handle/11683/80826 | |
| 942 | |c CF | ||