Relationship of the Structure and the Effective Diffusion Properties of Porous Zinc- and Copper-Containing Calcium Phosphate Coatings; Inorganic Materials: Applied Research; Vol. 9, iss. 3

Bibliografski detalji
Parent link:Inorganic Materials: Applied Research
Vol. 9, iss. 3.— 2018.— [P. 451-459]
Autori kompanije: Национальный исследовательский Томский политехнический университет Инженерная школа новых производственных технологий Отделение материаловедения, Национальный исследовательский Томский политехнический университет Исследовательская школа физики высокоэнергетических процессов
Daljnji autori: Nazarenko N. N. Nelli Nikolaevna, Knyazeva A. G. Anna Georgievna, Komarova E. G. Ekaterina Gennadjevna, Sedel'nikova M. B. Maria Borisovna, Sharkeev Yu. P. Yury Petrovich
Sažetak:Title screen
The morphology and the structure of zinc- or copper-containing calcium phosphate coatings deposited by the microarc oxidation (MAO) method at different voltages on pure titanium and low-modulus Ti-40 wt % Nb alloy substrates are investigated. The morphology of the MAO coatings on both substrates is composed of sphere-shaped structural elements 8-42 μm in size and pores 1-15 μm in size. When the process voltage is increased from 200 to 300 V, these structural elements grow and partially destruct. It is ascertained that the MAO voltage increase leads to the linear increase in the surface porosity of the coatings from 14 to 24%. It is established that the effective diffusion coefficients of the model biological fluid in porous coatings vary from 0.85 × 10-10 to 9.0 × 10-10 m2/s. Under the increase in the structure element size, the effective diffusion coefficient of the model biological fluid increases in the MAO coatings deposited on a titanium substrate and decreases in those deposited on Ti-40 wt % Nb alloy. The observed difference is related to the increase in the crystalline phase fraction.
Режим доступа: по договору с организацией-держателем ресурса
Jezik:engleski
Izdano: 2018
Teme:
Online pristup:https://doi.org/10.1134/S2075113318030243
Format: Elektronički Poglavlje knjige
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=659973

MARC

LEADER 00000naa0a2200000 4500
001 659973
005 20250328132758.0
035 |a (RuTPU)RU\TPU\network\28817 
090 |a 659973 
100 |a 20190410d2018 k||y0rusy50 ba 
101 0 |a eng 
102 |a US 
135 |a drcn ---uucaa 
181 0 |a i  
182 0 |a b 
200 1 |a Relationship of the Structure and the Effective Diffusion Properties of Porous Zinc- and Copper-Containing Calcium Phosphate Coatings  |f N. N. Nazarenko [et al.] 
203 |a Text  |c electronic 
300 |a Title screen 
320 |a [References: 16 tit.] 
330 |a The morphology and the structure of zinc- or copper-containing calcium phosphate coatings deposited by the microarc oxidation (MAO) method at different voltages on pure titanium and low-modulus Ti-40 wt % Nb alloy substrates are investigated. The morphology of the MAO coatings on both substrates is composed of sphere-shaped structural elements 8-42 μm in size and pores 1-15 μm in size. When the process voltage is increased from 200 to 300 V, these structural elements grow and partially destruct. It is ascertained that the MAO voltage increase leads to the linear increase in the surface porosity of the coatings from 14 to 24%. It is established that the effective diffusion coefficients of the model biological fluid in porous coatings vary from 0.85 × 10-10 to 9.0 × 10-10 m2/s. Under the increase in the structure element size, the effective diffusion coefficient of the model biological fluid increases in the MAO coatings deposited on a titanium substrate and decreases in those deposited on Ti-40 wt % Nb alloy. The observed difference is related to the increase in the crystalline phase fraction. 
333 |a Режим доступа: по договору с организацией-держателем ресурса 
461 |t Inorganic Materials: Applied Research 
463 |t Vol. 9, iss. 3  |v [P. 451-459]  |d 2018 
610 1 |a электронный ресурс 
610 1 |a труды учёных ТПУ 
610 1 |a effective diffusion coefficient 
610 1 |a porosity 
610 1 |a microarc oxidation 
610 1 |a calcium phosphate coating 
610 1 |a commercial pure titanium 
610 1 |a эффективный коэффициент 
610 1 |a диффузия 
610 1 |a пористость 
610 1 |a микродуговое оксидирование 
610 1 |a фосфат кальция 
610 1 |a титан 
701 1 |a Nazarenko  |b N. N.  |g Nelli Nikolaevna 
701 1 |a Knyazeva  |b A. G.  |c Russian physicist  |c Professor of Tomsk Polytechnic University, doctor of physico-mathematical Sciences  |f 1962-  |g Anna Georgievna  |3 (RuTPU)RU\TPU\pers\32712  |9 16597 
701 1 |a Komarova  |b E. G.  |g Ekaterina Gennadjevna 
701 1 |a Sedel'nikova  |b M. B.  |g Maria Borisovna 
701 1 |a Sharkeev  |b Yu. P.  |c physicist  |c Professor of Tomsk Polytechnic University, Doctor of physical and mathematical sciences  |f 1950-  |g Yury Petrovich  |3 (RuTPU)RU\TPU\pers\32228  |9 16228 
712 0 2 |a Национальный исследовательский Томский политехнический университет  |b Инженерная школа новых производственных технологий  |b Отделение материаловедения  |3 (RuTPU)RU\TPU\col\23508 
712 0 2 |a Национальный исследовательский Томский политехнический университет  |b Исследовательская школа физики высокоэнергетических процессов  |c (2017- )  |3 (RuTPU)RU\TPU\col\23551 
801 2 |a RU  |b 63413507  |c 20190410  |g RCR 
856 4 |u https://doi.org/10.1134/S2075113318030243 
942 |c CF