Cita APA (7th ed.)

Rusin N. M., Skorentsev A. L. Aleksandr Leonidovich, & Kolubaev Е. А. Evgeny Aleksandrovich. (2017). Effect of Hot Densification on Tribotechnical Properties of Sintered (Al-12Si)-40Sn Alloy. 2017. https://doi.org/10.1063/1.5013863

Cita Chicago (17th ed.)

Rusin N. M., Skorentsev A. L. Aleksandr Leonidovich, i Kolubaev Е. А. Evgeny Aleksandrovich. Effect of Hot Densification on Tribotechnical Properties of Sintered (Al-12Si)-40Sn Alloy. 2017, 2017. https://doi.org/10.1063/1.5013863.

Cita MLA (9th ed.)

Rusin N. M., et al. Effect of Hot Densification on Tribotechnical Properties of Sintered (Al-12Si)-40Sn Alloy. 2017, 2017. https://doi.org/10.1063/1.5013863.