Direct Alloying of Steel with Nickel Concentrate

Chi tiết về thư mục
Parent link:IOP Conference Series: Materials Science and Engineering
Vol. 142 : Innovative Technologies in Engineering.— 2016.— [012067, 8 p.]
Tác giả chính: Nokhrina O. I. Olga Ivanovna
Tác giả của công ty: Национальный исследовательский Томский политехнический университет (ТПУ) Юргинский технологический институт (филиал) (ЮТИ) Кафедра металлургии и черных металлов (МЧМ)
Tác giả khác: Rozhikhina I. D., Proshunin I. E.
Tóm tắt:Title screen
A technology of alloying steel with nickel reduced from nickel concentrate is analysed and developed. Limits of reduction concentration areas are defined. An optimal composition of nickel concentrate pellets and a method of feeding them into the furnace are deduced from experiments. It is proved that when pellets made of nickel concentrate and coke are added into the charge during steel smelting by the technology of alloyed scrap remelting, nickel recovery achieves 92-95%. The technology was tested by smelting DSP-40 steel.
Ngôn ngữ:Tiếng Anh
Được phát hành: 2016
Những chủ đề:
Truy cập trực tuyến:http://dx.doi.org/10.1088/1757-899X/142/1/012067
http://earchive.tpu.ru/handle/11683/34751
Định dạng: Điện tử Chương của sách
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=650440
Miêu tả
Tóm tắt:Title screen
A technology of alloying steel with nickel reduced from nickel concentrate is analysed and developed. Limits of reduction concentration areas are defined. An optimal composition of nickel concentrate pellets and a method of feeding them into the furnace are deduced from experiments. It is proved that when pellets made of nickel concentrate and coke are added into the charge during steel smelting by the technology of alloyed scrap remelting, nickel recovery achieves 92-95%. The technology was tested by smelting DSP-40 steel.
DOI:10.1088/1757-899X/142/1/012067