Effect of the passivating coating type, particle size, and storage time on oxidation and nitridation of aluminum powders; Combustion, Explosion and Shock Waves; Vol. 42, № 2
| Parent link: | Combustion, Explosion and Shock Waves.— , 1965- Vol. 42, № 2.— 2006.— [P. 177-184] |
|---|---|
| その他の著者: | , , , |
| 要約: | Title screen Processes of nonisothermal oxidation, nitridation, and ageing of aluminum powders with different particle sizes (nano-sized powder, ASD-1 powder, and PAP-2 powder) are considered. Application of non-oxide coatings onto particles of aluminum nanopowders reduces their thermal stability. Owing to scale-shaped particles, the PAP-2 powder after long-time storage preserves high activity of oxidation and nitridation, which is commensurable with that of the aluminum nanopowder. The activity of the coarse ASD-1 powder consisting of spherical particles in terms of oxidation and nitridation is low and only slightly changes during ageing. Режим доступа: по договору с организацией-держателем ресурса |
| 言語: | 英語 |
| 出版事項: |
2006
|
| 主題: | |
| オンライン・アクセス: | http://dx.doi.org/10.1007/s10573-006-0036-4 |
| フォーマット: | 電子媒体 図書の章 |
| KOHA link: | https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=646887 |
| 要約: | Title screen Processes of nonisothermal oxidation, nitridation, and ageing of aluminum powders with different particle sizes (nano-sized powder, ASD-1 powder, and PAP-2 powder) are considered. Application of non-oxide coatings onto particles of aluminum nanopowders reduces their thermal stability. Owing to scale-shaped particles, the PAP-2 powder after long-time storage preserves high activity of oxidation and nitridation, which is commensurable with that of the aluminum nanopowder. The activity of the coarse ASD-1 powder consisting of spherical particles in terms of oxidation and nitridation is low and only slightly changes during ageing. Режим доступа: по договору с организацией-держателем ресурса |
|---|---|
| DOI: | 10.1007/s10573-006-0036-4 |