Ultrasonic Surface Treatment of Titanium Alloys. The Submicrocrystalline State; IOP Conference Series: Materials Science and Engineering; Vol. 91: VI International Scientific Practical Conference on Innovative Technologies and Economics in Engineering, Yurga, Russia, 21-23 May 2015

書目詳細資料
Parent link:IOP Conference Series: Materials Science and Engineering
Vol. 91: VI International Scientific Practical Conference on Innovative Technologies and Economics in Engineering, Yurga, Russia, 21-23 May 2015.— 2015.— [012040, 6 p.]
企業作者: Национальный исследовательский Томский политехнический университет (ТПУ) Институт неразрушающего контроля (ИНК) Кафедра оборудования и технологии сварочного производства (ОТСП)
其他作者: Klimenov V. A. Vasily Aleksandrovich, Vlasov V. A., Borozna V. Yu. Vyacheslav Yurievich, Klopotov A. A.
總結:Title screen
The paper presents the results of the research on improvement of physical-and mechanical properties of titanium alloys VT1-0 and VT6 by modification of surfaces using ultrasonic treatment, and a comprehensive study of the microstructure and mechanical properties of modified surface layers. It has been established that exposure to ultrasonic treatment leads to formation in the surface layer of a structure with an average size of elements 50 x100 nm, depending on the brand of titanium alloy.
Режим доступа: по договору с организацией-держателем ресурса
語言:英语
出版: 2015
叢編:Innovative technologies for producing and machining materials in mechanical engineering
主題:
在線閱讀:http://dx.doi.org/10.1088/1757-899X/91/1/012040
http://earchive.tpu.ru/handle/11683/20002
格式: 電子 Book Chapter
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=644436
實物特徵
總結:Title screen
The paper presents the results of the research on improvement of physical-and mechanical properties of titanium alloys VT1-0 and VT6 by modification of surfaces using ultrasonic treatment, and a comprehensive study of the microstructure and mechanical properties of modified surface layers. It has been established that exposure to ultrasonic treatment leads to formation in the surface layer of a structure with an average size of elements 50 x100 nm, depending on the brand of titanium alloy.