Выделение титана из титаномагнетитовой руды

Bibliographic Details
Parent link:Перспективы развития фундаментальных наук=Prospects of Fundamental Sciences Development: сборник научных трудов XV Международной конференции студентов, аспирантов и молодых ученых, г. Томск, 24-27 апреля 2018 г./ Национальный исследовательский Томский политехнический университет (ТПУ) ; под ред. И. А. Курзиной, Г. А. Вороновой.— , 2018
Т. 2 : Химия.— 2018.— [С. 234-236]
Main Author: Орлов В. В.
Corporate Author: Национальный исследовательский Томский государственный университет (ТГУ)
Other Authors: Медведев Р. О. (727), Амеличкин И. В., Сачков В. И.
Summary:Заглавие с экрана
In this paper, we study the possibility of obtaining iron and titanium-vanadium concentrates with highest contents of iron and titanium, respectively, through hydrometallurgical processing of the titanomagnetite ores of the Chineisk deposit. Ammonium fluoride concentration was varied from 0.08 mol/L to 4.2 mol/L with the other fixed parameters. It was shown that optimum ammonium fluoride concentration for leaching the ore is 0.42 mol/L. The acidity of solution was changed by adding of hydrofluoric acid with varied concentration (from 0.86 mol/L to 4.07 mol/L) to ammonium fluoride solution with fixed concentration of 0.42 mol/L. The best results (degree of titanium extraction = 63.7%) were obtained when using a solution of hydrofluoric acid with concentration 4.07 mol/L.
Published: 2018
Subjects:
Online Access:http://earchive.tpu.ru/handle/11683/50777
Format: Electronic Book Chapter
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=627552
Description
Summary:Заглавие с экрана
In this paper, we study the possibility of obtaining iron and titanium-vanadium concentrates with highest contents of iron and titanium, respectively, through hydrometallurgical processing of the titanomagnetite ores of the Chineisk deposit. Ammonium fluoride concentration was varied from 0.08 mol/L to 4.2 mol/L with the other fixed parameters. It was shown that optimum ammonium fluoride concentration for leaching the ore is 0.42 mol/L. The acidity of solution was changed by adding of hydrofluoric acid with varied concentration (from 0.86 mol/L to 4.07 mol/L) to ammonium fluoride solution with fixed concentration of 0.42 mol/L. The best results (degree of titanium extraction = 63.7%) were obtained when using a solution of hydrofluoric acid with concentration 4.07 mol/L.