Clean and efficient extraction of copper ions and deposition as metal

Bibliographic Details
Parent link:Resource-Efficient Technologies: electronic scientific journal/ National Research Tomsk Polytechnic University (TPU).— , 2015-.— 2405-6537
Vol. 1, Iss. 1.— 2015.— [P. 28-33]
Main Author: Elsentriecy H. H. Hassan
Other Authors: Jalbout A. F. Abraham, Gervasio D. F. Dominic
Summary:Title screen
A simple, clean and efficient one-pot process is offered as an alternative to the conventional complex processing presently used to extract copper ions from copper containing materials, like copper concentrate or slag, and to form copper metal. The alternative process uses a eutectic molten salt of potassium chloride, sodium chloride and zinc chloride as the reaction fluid which is recyclable, low in cost, environmentally benign, low melting (melting point 204°), high boiling (vapor pressure is only a few psi at 800°) and chemically, thermally and physically stable. The metal completely dissolves out of copper concentrate or slag in the aerobic eutectic molten chloride salt in a graphite or glassy carbon pot, which serves as a cathode, with a graphite anode, to reduce the metal ions to metal which sinks to the bottom of the graphite pot. The total efficiency for extraction and deposition is virtually 100% as determined by elemental and gravimetric analyses.
Published: 2015
Subjects:
Online Access:http://earchive.tpu.ru/handle/11683/50191
Format: Electronic Book Chapter
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=553601
Description
Summary:Title screen
A simple, clean and efficient one-pot process is offered as an alternative to the conventional complex processing presently used to extract copper ions from copper containing materials, like copper concentrate or slag, and to form copper metal. The alternative process uses a eutectic molten salt of potassium chloride, sodium chloride and zinc chloride as the reaction fluid which is recyclable, low in cost, environmentally benign, low melting (melting point 204°), high boiling (vapor pressure is only a few psi at 800°) and chemically, thermally and physically stable. The metal completely dissolves out of copper concentrate or slag in the aerobic eutectic molten chloride salt in a graphite or glassy carbon pot, which serves as a cathode, with a graphite anode, to reduce the metal ions to metal which sinks to the bottom of the graphite pot. The total efficiency for extraction and deposition is virtually 100% as determined by elemental and gravimetric analyses.