Интерметаллическое соединение Ni-Al как несущая основа для твердооксидных топливных элементов
| Parent link: | Перспективы развития фундаментальных наук=Prospects of fundamental sciences development: сборник научных трудов IX Международной конференция студентов и молодых ученых, г. Томск, 24-27 апреля 2012 г./ Национальный исследовательский Томский политехнический университет (ТПУ). [С. 130-132].— , 2012 |
|---|---|
| Main Author: | |
| Corporate Authors: | , |
| Other Authors: | , , |
| Summary: | Заглавие с экрана The results of application of self-propagating high temperature synthesis for the manufacture of porous Ni-Al supports of solid oxide fuel cells are presented. The effect of synthesis conditions and raw materialsmixture on the phase composition, microstructure, porosity, gas permeability, corrosion resistance and otherproperties of the Ni-Al samples is investigated. It is shown the possibility of forming on the surface of porous Ni-Al supports of solid oxide fuel cells with the structure of Ni-ZrO2:Y2O3 anode / ZrO2:Y2O3 electrolyte / La0.8Mn0.2SrO3 cathode, ensuring the power density of 400 mW/cm2at temperature 800°С. |
| Published: |
2012
|
| Series: | Физика |
| Subjects: | |
| Online Access: | http://www.lib.tpu.ru/fulltext/c/2012/C21/040.pdf |
| Format: | Electronic Book Chapter |
| KOHA link: | https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=236540 |
| Physical Description: | 1 файл(640 Кб) |
|---|---|
| Summary: | Заглавие с экрана The results of application of self-propagating high temperature synthesis for the manufacture of porous Ni-Al supports of solid oxide fuel cells are presented. The effect of synthesis conditions and raw materialsmixture on the phase composition, microstructure, porosity, gas permeability, corrosion resistance and otherproperties of the Ni-Al samples is investigated. It is shown the possibility of forming on the surface of porous Ni-Al supports of solid oxide fuel cells with the structure of Ni-ZrO2:Y2O3 anode / ZrO2:Y2O3 electrolyte / La0.8Mn0.2SrO3 cathode, ensuring the power density of 400 mW/cm2at temperature 800°С. |