Features of change of mechanical properties of precipitation hardening alloy 47ХНМ at hardening and ageing; Bulletin of the Tomsk Polytechnic University; Vol. 311, № 2

Dades bibliogràfiques
Parent link:Bulletin of the Tomsk Polytechnic University/ Tomsk Polytechnic University (TPU).— , 2006-2007
Vol. 311, № 2.— 2007.— [P. 114-116]
Altres autors: Mukazhanov E. B., Skakov M. K., Isaeva Zh. M., Erbolatuly D.
Sumari:Заглавие с титульного листа
Электронная версия печатной публикации
Mechanical properties of nickel-chromic austenitic alloy 47ХНМ have been studied. It was shown that at increase of heating time for hardening the deforming pressures fall, plasticity grows that is connected with dissolution of excess a-phase. In order to obtain high strength properties with minimum level of elastic imperfections the thermal processing of alloy should be carried out in temperature range 650...750 °С, and time of ageing should be from 8 to 20 h depending on temperature of ageing
Idioma:anglès
Publicat: 2007
Col·lecció:Mathematics and mechanics.Physics
Matèries:
Accés en línia:http://www.lib.tpu.ru/fulltext/v/Bulletin_TPU/2007/v311eng/i2/29.pdf
Format: MixedMaterials Electrònic Capítol de llibre
KOHA link:https://koha.lib.tpu.ru/cgi-bin/koha/opac-detail.pl?biblionumber=182951

MARC

LEADER 00000nla2a2200000 4500
001 182951
005 20231031171430.0
035 |a (RuTPU)RU\TPU\book\198324 
035 |a RU\TPU\book\198115 
090 |a 182951 
100 |a 20100629d2007 k y0rusy50 ca 
101 1 |a eng  |c rus 
102 |a RU 
135 |a drnn ---uucaa 
200 1 |a Features of change of mechanical properties of precipitation hardening alloy 47ХНМ at hardening and ageing  |b Electronic resource  |f E. B. Mukazhanov [et al.] 
203 |a Text  |c electronic 
215 |a 1 файл (486 Кб) 
225 1 |a Mathematics and mechanics.Physics 
230 |a Электронные текстовые данные (1 файл : 486 Кб) 
300 |a Заглавие с титульного листа 
300 |a Электронная версия печатной публикации 
320 |a [Bibliography: p. 116 (3 titles)] 
330 |a Mechanical properties of nickel-chromic austenitic alloy 47ХНМ have been studied. It was shown that at increase of heating time for hardening the deforming pressures fall, plasticity grows that is connected with dissolution of excess a-phase. In order to obtain high strength properties with minimum level of elastic imperfections the thermal processing of alloy should be carried out in temperature range 650...750 °С, and time of ageing should be from 8 to 20 h depending on temperature of ageing 
337 |a Adobe Reader 
461 1 |0 (RuTPU)RU\TPU\book\169973  |t Bulletin of the Tomsk Polytechnic University  |f Tomsk Polytechnic University (TPU)  |d 2006-2007 
463 1 |0 (RuTPU)RU\TPU\book\197892  |x 1684-8519  |t Vol. 311, № 2  |v [P. 114-116]  |d 2007  |p 153 p. 
610 1 |a mechanical properties 
610 1 |a precipitation hardening alloys 
610 1 |a hardening 
610 1 |a ageing 
610 1 |a plasticity 
610 1 |a high strength properties 
610 1 |a thermal processing 
610 1 |a электронный ресурс 
675 |a 538.9:621.785.6  |v 3 
701 1 |a Mukazhanov  |b E. B. 
701 1 |a Skakov  |b M. K. 
701 1 |a Isaeva  |b Zh. M. 
701 1 |a Erbolatuly  |b D. 
801 1 |a RU  |b 63413507  |c 20090623  |g PSBO 
801 2 |a RU  |b 63413507  |c 20120418  |g PSBO 
856 4 |u http://www.lib.tpu.ru/fulltext/v/Bulletin_TPU/2007/v311eng/i2/29.pdf 
942 |c CF